Bitumen 30/40
Test | Methodology | Value |
---|---|---|
Density | ASTM D-7 | 1/01 – 1/06 |
Penetration Rate at 25°C | ASTM D-5 | 30-40 |
Softening Point ⁰C | ASTM D-36 | 55-63 |
Ductility at 25°C (cm) – Min | ASTM D-113 | 100 |
Flash Point °C – Min | ASTM D-92 | 250 |
Solubility in disulfide %wt | ASTM D-4 | 99/5 |
Satin Test | AASHTO T 102 | Negative |
Weight Loss by Heating %wt – MAX | ASTM D-6 | 0/2 |
Penetration Loss by Heating % – MAX | ASTM D-6 – D-5 | 20 |